Ikhwalithi Enhle Ithoni Ye-Invar Permalloy Inconel 625 718 Ni80cr20 Monel Inkoloy Pure Nickel Superalloy Plate Steel Plates Nickel Alloy Sheet
Incazelo emfushane:
I-Inconel625 alloy (UNS 6625) iyingxubevange ye-austenitic superheat resistant ikakhulukazi eyakhiwe nge-nickel, enezakhiwo ezinhle kakhulu zokumelana ne-oxidation nokumelana nokugqwala.
Siqhubeka nomgomo "wokuqala wekhwalithi, isevisi kuqala, ukuthuthukiswa okuqhubekayo kanye nokuqanjwa kabusha ukuze sihlangabezane namakhasimende" kwezokuphatha kanye "nokungabi nasici, izikhalazo ezingenakho" njengenhloso yekhwalithi.Ukuze sibe nosizo lwethu oluhle, sinikeza izimpahla kuyilapho sisebenzisa ikhwalithi ephezulu enhle ngentengo efanelekile yeTon Yekhwalithi Enhle ye-Invar Permalloy Inconel 625 718 Ni80cr20 Monel Incoloy Pure Nickel Superalloy Plate Steel Plates Nickel Alloy Sheet, Njengomkhiqizi ohamba phambili nomthumeli ngaphandle, thina ujabulele idumela elihle ezimakethe zamazwe ngamazwe, ikakhulukazi eMelika naseYurophu, ngenxa yekhwalithi yethu ephezulu namanani aphansi.
Siqhubeka nomgomo "wokuqala wekhwalithi, isevisi kuqala, ukuthuthukiswa okuqhubekayo kanye nokuqanjwa kabusha ukuze sihlangabezane namakhasimende" kwezokuphatha kanye "nokungabi nasici, izikhalazo ezingenakho" njengenhloso yekhwalithi.Ukuze sibe nosizo oluhle, sinikeza izimpahla ngenkathi sisebenzisa ikhwalithi ephezulu enhle ngentengo ephusileI-China Nickel Alloy Plate kanye ne-alloy Plate, sihlala sigcina isikweletu sethu nenzuzo efanayo kumakhasimende ethu, sigcizelela isevisi yethu yekhwalithi ephezulu ekuhambiseni amakhasimende ethu.njalo wamukela abangani bethu namakhasimende ukuthi beze bazovakashela inkampani yethu futhi baqondise ibhizinisi lethu, uma unentshisekelo ngemikhiqizo yethu, ungathumela imininingwane yakho yokuthenga ku-inthanethi, futhi sizokuthinta ngokushesha, sigcina ukubambisana kwethu okuqotho nesifiso sethu. konke okuseceleni kwakho konke kuhamba kahle.
I-Inconel625 alloy (UNS 6625) iyingxubevange ye-austenitic superheat resistant ikakhulukazi eyakhiwe nge-nickel, enezakhiwo ezinhle kakhulu zokumelana ne-oxidation nokumelana nokugqwala.Ilungele izinkambu eziningi ezihlanganisa izindawo zenjini yendiza yendiza, ezondiza, kanye nokucutshungulwa kwamakhemikhali.Emazingeni okushisa aphansi njengo-2000 degrees Fahrenheit (1093 degrees Celsius), le alloy futhi ikhombisa ukumelana nokukhathala okumangalisayo.Amandla we-625 alloy avela kumphumela oqinisayo we-molybdenum ne-niobium izixazululo eziqinile eziqukethwe ku-nickel chromium alloy.Lezi zakhi ziphinde zinikeze i-alloy ukumelana nokugqwala okuhle kakhulu.Nakuba le ngxubevange yakhelwe amandla ezindaweni ezinezinga lokushisa eliphezulu, inhlanganisela yayo ephezulu yengxubevange iyenza ikwazi ukubekezelela ukugqwala okujwayelekile kanye nezindawo eziningi ezixutshwa ne-oxidizing nezingezona oxidizing.Okuqukethwe kwe-chromium ne-molybdenum kunikeza ingxubevange ukumelana okuhle kakhulu namabala okugqwala okubangelwa izici ze-ion chloride: Okuqukethwe kwe-nickel ephezulu kuthuthukisa ukumelana kwama-alloys ekuqhekekeni kwe-chloride stress corrosion
ASTM B443/ASME SB-443,ASTM B444/ASME SB-444,ASTM B366/ASME SB-366,ASTM B446/ASME SB-446,ASTM B564/ASME SB-564
C | Mn | Ni | Si | P | Cr | S | Fe | Al | Ti | Nb | Co | Mo |
≤0.01 | ≤0.50 | ≥58 | ≤0.50 | ≤0.015 | 20.0-23.0 | ≤0.015 | ≤5.0 | ≤0.4 | ≤0.4 | 3.15–4.15 | ≤1.0 | 8.0-10.0 |
Ukuminyana | I-Melting Point |
8.44g/cm3 | 1290-1350 ℃ |
Amandla Okuqina | Isivuno Amandla | Ukwelula | Ukuqina |
σb≥758Mpa | σb≥379Mpa | δ≥30% | I-HB150-220 |
I-ERNiCrMo-3 ENiCrMo-3
Supply Product
Ipuleti, I-Strip, Ibha, Intambo, Ukuqamba, Induku Ebushelelezi, Izinto Zokushisela, I-Flange, njll. Futhi singacutshungulwa ngokuya ngomdwebo
Izingxenye zezinqubo zamakhemikhali ezinto eziphilayo eziqukethe ama-chloride, ikakhulukazi uma usebenzisa ama-catalysts e-acidic chloride;Amathangi okupheka nokuhlanza asetshenziswa embonini ye-pulp nephepha;Umbhoshongo wokumuncwa, i-reheater, i-flue gas inlet baffle, ifeni (emanzi), i-agitator, i-guide plate, kanye ne-flue kusistimu ye-flue gas desulfurization;Isetshenziselwa ukukhiqiza imishini kanye nezingxenye ezisetshenziswa ezindaweni zegesi ene-asidi;I-acetic acid kanye ne-acetic anhydride reaction generator;i-sulfuric acid condenser;Imishini yokwenza imithi;Izimboni nemikhiqizo enjengamajoyinti okunweba ama-bellows.
I-INCONEL 625 i-austenitic superheat resistant alloy ngokuyinhloko eyakhiwe nge-nickel.Isuka ekuqiniseni izixazululo ze-molybdenum ne-niobium eziqinile eziqukethwe ku-nickel chromium alloys, inamandla aphakeme kakhulu kanye nokumelana nokukhathala okungavamile emazingeni okushisa aphansi afika ku-1093 ℃, futhi isetshenziswa kabanzi embonini yezindiza.Nakuba le ngxubevange yenzelwe amandla ezindaweni ezinokushisa okuphezulu, okuqukethwe kwayo okuphezulu kwe-chromium ne-molybdenum kunokumelana okuphezulu nemidiya yokugqwala, ukusuka endaweni ene-oxidizing kuya ezindaweni ezigqwalile ezijwayelekile, ezinokumelana okuphezulu nezindawo zokugqwala nokugqwala, okubonisa ukumelana nokugqwala okuhle kakhulu. izici.I-INCONEL 625 futhi inokumelana nokugqwala okuqinile ngokumelene nemidiya engcolile ye-chloride njengamanzi olwandle, amanzi ashisayo, usawoti ongathathi hlangothi, namanzi anosawoti.
Siqhubeka nomgomo "wokuqala wekhwalithi, isevisi kuqala, ukuthuthukiswa okuqhubekayo kanye nokuqanjwa kabusha ukuze sihlangabezane namakhasimende" kwezokuphatha kanye "nokungabi nasici, izikhalazo ezingenakho" njengenhloso yekhwalithi.Ukuze sibe nosizo lwethu oluhle, sinikeza izimpahla kuyilapho sisebenzisa ikhwalithi ephezulu enhle ngentengo efanelekile yeTon Yekhwalithi Enhle ye-Invar Permalloy Inconel 625 718 Ni80cr20 Monel Incoloy Pure Nickel Superalloy Plate Steel Plates Nickel Alloy Sheet, Njengomkhiqizi ohamba phambili nomthumeli ngaphandle, thina ujabulele idumela elihle ezimakethe zamazwe ngamazwe, ikakhulukazi eMelika naseYurophu, ngenxa yekhwalithi yethu ephezulu namanani aphansi.
Ikhwalithi EnhleI-China Nickel Alloy Plate kanye ne-alloy Plate, sihlala sigcina isikweletu sethu nenzuzo efanayo kumakhasimende ethu, sigcizelela isevisi yethu yekhwalithi ephezulu ekuhambiseni amakhasimende ethu.njalo wamukela abangani bethu namakhasimende ukuthi beze bazovakashela inkampani yethu futhi baqondise ibhizinisi lethu, uma unentshisekelo ngemikhiqizo yethu, ungathumela imininingwane yakho yokuthenga ku-inthanethi, futhi sizokuthinta ngokushesha, sigcina ukubambisana kwethu okuqotho nesifiso sethu. konke okuseceleni kwakho konke kuhamba kahle.